C | .05 - .15 | MN | 1.0- 2.0 |
---|---|---|---|
P | .4 | S | .03 |
Si | .4 | Cr | 19.0 - 21.0 |
Ni | 9.0 - 11.0 | Co | bal |
W | 14.0 - 16.0 |
Haynes 25™ alloy is the strongest of all the fabricable cobalt alloys. It has an excellent temperature strength and oxidation resistance to 2000 °F. However, Haynes 25™ cobalt alloy is hot formable between 1900 ≥F- 2300 °F. In addition, it is better to cold-work alloy L605 for bending, spinning and drawing component processes.
Haynes alloy L605 is used for diverse types of industrial applications, including: